search  current discussion  categories  techniques - stains 

regarding underglazes post--ooops!

updated fri 9 oct 98

 

Greg Lamont on thu 8 oct 98

Richard, et al,

I realized after I pushed the "send" button that I misspoke. I meant to
say just the opposite-- that I've only used the underglaze recipe on
greenware--NOT on bisqueware. Sorry.

Greg

Greg Lamont
3011 Northwood Dr.
Ames, Iowa 50010-4750
515/233-3442
gdlamont@iastate.edu