search  current discussion  categories  glazes - cone 8-10 

rhodes white glaze, cone 9-10

updated fri 9 oct 98

 

Stacey Lennard on wed 7 oct 98

Hi,

I am wondering if anybody could help me reformulate this glaze so that it will b

The glaze is Rhode's White. It originally called for K-200 Feldspar but I could
Here is the recipe which I have used:

Dolomite 18.73
Gerstley Borate 6.37
Whiting 4.16
G-200 41.61
EPK 20.81
Flint 8.32
(Superpax 5.00)
(Bentonite 2.00)

Thanks Very Much,
Steve Saxenian
Lenny@art.umass.edu

Milton Markey on thu 8 oct 98

In a message dated 98-10-07 09:00:28 EDT, you write:

> I am wondering if anybody could help me reformulate this glaze so that it
> will b
>
Could you finish the question please? I think the end of your statement got
chopped off by the EMail devils!

Milton MiltonsLin@AOL.COM