Hi again folks,

Anyone know of a REALLY satiny, buttery white raku glaze, preferably around
^07? I have tried almost every formula I can find and still haven't found THE
PERFECT white. I would like to find one using Cornwall Stone, which gives
that "thick buttery" feel. Am testing more today with fingers crossed.
thanks guys,
Karen in Sonoma

cyberscape on tue 15 dec 98

Karen,

Try this one

Fat White Raku

Frit 3134 82
Ball Clay 9
Zircopax 9

Harvey Sadow