Laurie Friedlander on fri 4 sep 98
Someone told me of a source for inexpensive/ used silicon carbide shelves, but
I don't recall info. Does anyone out there know of such a source? I have
called one such in Texas from ad in Ceramics Monthly, but would like to know
if there are others, especially closer to N.Y. Thanks! -Laurie
Kelley Webb Randel on sat 5 sep 98
Hey All!
Does anyone have a source for cheap kiln shelves near Missouri?
Thanks,
Kelley Webb Randel
J. D. Walker on tue 8 sep 98
kelly,
try L&R out of Nixa, Mo. 12x24's are about $30.00 ea. Ask for Jerry.
Or you Can call Brackers in Lawrance,KS. They carry Thorley Shelves, at
about $34.00 for the 12x24's
jeff walker
where this last art show was OK but rather slow on a day by day take.
-----Original Message-----
From: Kelley Webb Randel
To: CLAYART@LSV.UKY.EDU
Date: Saturday, September 05, 1998 11:41 AM
Subject: Re: Source for cheap kiln shelves?
>----------------------------Original message----------------------------
>Hey All!
>Does anyone have a source for cheap kiln shelves near Missouri?
>Thanks,
>Kelley Webb Randel
>
| |
|