Wendy Moore on thu 5 nov 98
Glaze Gurus:
I have a question... Is it possible to achieve a "good" yellow using
strontium instead of barium? We've been doing some testing to lower our
barium use in a class studio situation. We have not had any luck with
yellows. We're looking for ^10 reduction, but would be interested in
any way to achieve this. We'll continue to test but if anyone has any
good places to start.... we'd appreciate it. TIA
Wendy Moore, the Apron Lady
In Crispy, brisk, I think it's almost time for a jacket, Michigan
| |
|