Hello everyone, Here is a blue glaze. It is a ^6 oxidation, but I have
used it in ^10 reduction and it turned out great.

Pinnell Strontium Matt

Lithium Carb. 1.0
Strontium Carb. 20.0
Neph Sy. 60.0
Ball 10.0
Flint 9.0

Wheathered Bronze
Titanium Diox. 5.0
Copper Carb. 5.0

Wheathered Blue
Cobalt Carb. .15
Copper Carb. 4.0

Happy Glazing, Jennifer in Alpine, TX


********************************