search  current discussion  categories  glazes - specific colors 

mottled matte blue

updated fri 22 jan 99

 

Jan Adams on thu 21 jan 99

Noticed that people are looking for the blues again, so I thougt I'd throw =
in
this request. I'm looking for a matte blue, probably between =5E6 and =
=5E10. I
know it fires in oxidation. It's a mottled, soft light to med. blue. Areas=
of
lighter and darker blue seem to float at random....I've seen the glaze, and
tried to figure out what would make it. There is a lot of white in it, and =
it
mostly seems to make up the background. Any suggestions appreciated. =
Thanks,
Jan