Hello Molly, Try making a gasket from thin rubber sheeting, you shouldn't
need anything thicker than 1-2mm. If you can't find any, then try a bead of
rubber or silicone gasket goo as sold at your local motorbike or car parts
place.
Good Luck, wish I had a pugmill sometimes...