Pat Schurr on thu 21 jan 99
Has anyone used the Synthetic Ash glaze receipes in Phil Rogers's book
"Ash Glazes?" I am interested in which ones you may have tried and what
the results were. Thank you.
Pat Schurr
Burned Earth Studio
Oak Ridge, NC
Lee Love on sat 23 jan 99
----- Original Message -----
From: Pat Schurr :
>Has anyone used the Synthetic Ash glaze receipes in Phil Rogers's book
>"Ash Glazes?"
Yes, I use the synthetic Nuka. It is interesting over temmoku.
/(o\' Lee In Saint Paul, Minnesota USA 0
\o)/' mailto:Ikiru@Kami.com ICQ# 20586182
' http://www.millcomm.com/~leelove/taiko.html
Karin Hurt on fri 9 mar 01
Would anyone be willing to share a recipe? Can it be fired in oxidation or
does it need to be fired in reduction?
Thanks
Karin
| |
|