Veena Raghavan on mon 25 jan 99
---------- Forwarded Message ----------
From: Veena Raghavan, 75124,2520
TO: Ceramic Arts Discussion List, INTERNET:CLAYART@LSV.UKY.EDU
DATE: 01-22-99 01:17 AM
RE: Copy of: Re: Iron reds/Randy's Red
Did anyone ever reply to the question of how much crocus martis should be
added to Randy's Red to enhance the red. If so, I missed it and would
really appreciate if it could be posted again. We use Randy's in our
studio, but although we get a fair amount of rust red on the inside, the
outside can often be quite dull. Would love to be able to get more red.
Thanks in advance.
Veena Raghavan
75124.2520@compuserve.com
Barbara Lewis on mon 25 jan 99
Veena: You might be having e-mail problems because you must not have gotten
the e-mail I sent to you privately. Use half crocus martis and half RIO in
Randy's Red. So for instance, if the recipe calls for 80 grams of RIO, use
40 crocus and 40 RIO. Good luck, Barbara
At 02:15 PM 1/25/99 EST, you wrote:
>----------------------------Original message----------------------------
>
>---------- Forwarded Message ----------
>
>From: Veena Raghavan, 75124,2520
>TO: Ceramic Arts Discussion List, INTERNET:CLAYART@LSV.UKY.EDU
>DATE: 01-22-99 01:17 AM
>
>RE: Copy of: Re: Iron reds/Randy's Red
>
>Did anyone ever reply to the question of how much crocus martis should be
>added to Randy's Red to enhance the red. If so, I missed it and would
>really appreciate if it could be posted again. We use Randy's in our
>studio, but although we get a fair amount of rust red on the inside, the
>outside can often be quite dull. Would love to be able to get more red.
>Thanks in advance.
>Veena Raghavan
>75124.2520@compuserve.com
>
Wellspring Clayworks
5412 Well Spring Road
La Plata, MD 20646
blewis@crosslink.net
| |
|