Stacey A Lennard on wed 3 feb 99
Here is a recipe for a cone 10 white, glossy glaze.
I am having trouble with it: it develops pinholes
when applied medium to thick on white
stoneware. It seems to develop a flawless surface
on darker, iron bearing stoneware. Any ideas on how
to change it so that it works on the white stoneware?
Potash feldspar 67.7 %
Pearl Ash 3.7
Dolomite 11.4
Flint 7.4
Zircopax 5.5
Bentonite 4.3
Thanks,
Steve Saxenian
| |
|