Lesley Alexander on wed 3 feb 99
Hi Ellen, Laguna Clay is one supplier that has stands and wires for
glazing beads. They used to have a thinner nichrome wire for beads with
smaller holes as well; These one could just hang between any bisqued pieces
or fire brick, not leaving too much distance or they would sag and the
beads would slide! Perhaps someone has a new source for that thinner wire.
Meanwhile, Laguna has outlets in Denver, NY and Ohio as well as Los
Angeles. For Denver try (800) 452-4862; NY (800) 762-4354; Ohio (800)
452-4862. Good luck! Lesley in Santa Barbara CA.
| |
|