=3EI have sprayed glaze for years and often found small =22goose bump=22 =
like
=3Ebubbles forming just about at the point when I feel I have reached a
=3Esatisfactory thickness. I know those =22goose bumps=22 are small air
=3Ebubbles but am not sure why they form.
=3E
=3EAny ideas?
=3E
I had that problem a couple of years ago. .Too much water in the glaze . =
When
the pott can=60t take up any more water it stays at the surface of the =
glaze .
I have about 35 - 40=25 water in the glaze, depending on what glaze it is, =
today
and air-pressure at 0,10 - 0,20 kilo and now it works fine.

Take Care
Isak Isaksson