BCWBTile@aol.com on sat 6 feb 99

Hi! We're interested in finding out about pigments others have found useful
to use on an already-glazed surface, and the best sources for aquiring these.
We're especially interested in water-based pigments that would be fired in the
018-016 cone range. Any help or information would be greatly appreciated.
Thanks.

Paul Lewing on mon 8 feb 99

Look up my article "China Paint; the Ultimate in Low-Fire" in Ceramics
Monthly from Feb. 1995. It has quite a bit about silk-screening on
tile.
Paul Lewing, Seattle, where we're going for our fourth straight month
of record rainfall.