Tracy or Joy Gunderman on mon 8 feb 99
Jeff Lawrence asked Ferro about Hommel 294 replacement and was told Ferro
#3271 but that was not made for 20 years and they offered no numbers.
John Conrad's "Advanced Ceramic Manual" does not list that Hommel number
but lists Ferro 3271 as:
Na2O .486
K2O .514
B2O3 .768
SiO2 2.25
Mol Wt 247.9
Fusion degC 810C
Hope this helps
Tracy Gunderman
| |
|