Marcia Kindlmann on mon 15 feb 99
Subject: High fire and low fire clays,how to keep separate
Hi Carolyn,
To not get these two clays mixed up for the glaze firing -- is there enough
room for separate (conspicuously labeled) shelves to keep these different pots
on? Or - only work on one kind at a time?
Another idea -- if your friend can get everyone to remember it -- make a mark
on the bottom of the leather hard pot as soon as it's trimmed, along with the
maker's signature.
Marcia in CT
| |
|