alligator re: lichen glaze

updated sat 6 mar 99

 

zahidi on fri 5 mar 99

"Piepenburg alligator "

This is a Raku glaze (06-04)
gerstley 4
Neph sye 1
Bone ash 2
Copper carb 1

zahidi@gs.verio.net
-----Original Message-----
From: Bacia Edelman
To: CLAYART@LSV.UKY.EDU
Date: Thursday, March 04, 1999 6:38 AM
Subject: Re: lichen glaze


----------------------------Original message----------------------------
>>I already deleted the Digest with the question . Someone, whose wife is a
weaver and uses some lichen in the woven work, asked if real lichen was used
in a glaze. No, it isn't because lichen is a combustible and would burn up
early in the firing. What it leaves behind might be strange: try it.
I have heard of "alligator glaze", a cone 04 glaze (don't have the recipe).
Take it from there.<<