search  current discussion  categories  kilns & firing - manufacturers 

skutt/enviro vent

updated wed 10 mar 99

 

gemini53 on tue 9 mar 99

I too am the proud owner of a Skutt 1027. I have been using it for a year =
now
with excellant results. I always shut off the vent whent the kiln shuts =
off. I
don't see any need for it to run and I do not want cool air pulled into the
kiln. And if I remember correctly, the instructions that came with the =
kiln
advise one to do so.
That's my two cents worth from NC, where mother nature can't decide if it is
spring or winter.
Sheron Roberts
Red Hawk Studios
Whiteville, NC
gemini53=40weblnk.net