Jim and Joan Warren on mon 15 mar 99
Hi Clayarters,
One of our Guild members asked me to ask any cone 10 saggar "fire-ers" out
there if they have a good stable glaze that withstands heavy smoke and heavy
reduction. A lot of glazes, especially the shino's she has tried seem to
bubble and blister with the heavy smoke reduction.
Thanks Joan Warren
| |
|