I have Insight5 cost about $120.00 From Digitalfire.com a great
website by the way.
I think they sell it through Axner Pottery 1 800 843 7057. At least
that was where I gave my credit card number last year. They gave out 30
day disks at NCECA last year so you could try it out. The program quit
working after 30 days if you didn't have the purchase code. The nice
thing about it is that you can split the screen and make incremental
weight changes or molecular changes on one side and see how it compares
to the original side by side.
The other one I have is called GlazeChem it is available as shareware
to download, then lyou send the developer a fee it you keep it. About
$30.00. there are things about this program I really like also. I like
the reports I can print on each glaze, not just the formula, but a
rundown on the chemicals, possible hazards, etc.
I use both.

--