Could someone please give me a sub for spodumene (or a rose by any
other name ?)
Superpax? Is this a sub for Tin Ox?
Could one call frit 3134 a high alkaline borrosilicate frit?
I feel like playing with feathering.
Toni in Durban South Africa wishing the tail end of summer would disappear into
COOL!

36 frit 3124
14 magnesium carbonate
20 neph sye
22 strontium
30 spodumene
20 EPK
26 whiting
24 superpax
2 bentonite
30 unwashed wood ash from fireplace

Of course it could be the result of whatever kind of wood my friend used
in her fireplace. This glaze by itself is not particularly
interesting. You should watch for excessive runs, but I've seldom had
the glaze run off the pots.
--