search  current discussion  categories  kilns & firing - misc 

fire bick companys/

updated sat 10 apr 99

 

Hank Ray on fri 9 apr 99

Hello there..
On the advice of a fellow clayarter i called a. p. green back.. and found out
that they have a price break at one pallet... 750 bricks.. the price then for
K-23's is $3.02
If you want four pallets .... 3000 bricks then the price goes to $2.59....

anybody from the oklahoma area need 1800 bricks,,we can go in together...
i'll go get them...

as for the national brand bricks i found out today.... that they used to be
called "KAISER" (spelling?) does that ring any bells....??????

pete over and out
Helllll@aol.com







In a message dated 4/8/99 11:52:34 AM !!!First Boot!!!, Helllll@AOL.COM
writes:

> ----------------------------Original message----------------------------
> Hello
>
> I called A. P. Green in Dallas today about buying IFB's, they quoted me $3.
> 49
> for k-23 and $3.88 for k-26...
>
> I found a place local here in Oklahoma City, that sells "NATIONAL" brand
....
>
> 23's for $2.43 and 26's for $3.15
>
> so i have two questions.. first doesn't the A. P. Green price seem high?
> and has anyone heard of "NATIONAL" ......