Ron Roy on thu 15 apr 99
Hi David,
I'm back from the New York workshop but snowed under with ClayArt mail and
glaze work. It went well - I have figured out how to teach calculation
quickly though. All you need to do is convince them it is not that
complicated - so I sepend the first hour telling them how simple it it -
like if I can do this anyone can. Well maybe not the whole truth but trying
to get potters to understand when they think they can't - well - makes the
job a lot harder.
I need the analysis for Pottery Craft frit # 2954 - described as a
calcium/borate frit.
Thanks for any help you can give.
Best regards, RR
Ron Roy
93 Pegasus Trail
Scarborough, Ontario
Canada M1G 3N8
Tel: 416-439-2621
Fax: 416-438-7849
Web page: http://digitalfire.com/education/people/ronroy.htm
musa on fri 16 apr 99
Hello Ron,
I noticed that your post is addressed to David, but I have the molecular
formula of the frit you are looking for, so forgive the eager reply:
Potterycrafts Calcium Borate Frit P2954:
CaO 1.00
Al2O3 0.097
Sio2 0.609
B2O3 1.5
Molecular Weight 207.1
Firing Range: 1050 - 1160 C
Greetings,
Musa.
-----Original Message-----
From: Ron Roy [SMTP:ronroy@total.net]
Sent: Thursday, April 15, 1999 12:54 PM
To: CLAYART@LSV.UKY.EDU
Subject: Re: Frit analysis needed
----------------------------Original message----------------------------
Hi David,
I'm back from the New York workshop but snowed under with ClayArt mail and
glaze work. It went well - I have figured out how to teach calculation
quickly though. All you need to do is convince them it is not that
complicated - so I sepend the first hour telling them how simple it it -
like if I can do this anyone can. Well maybe not the whole truth but trying
to get potters to understand when they think they can't - well - makes the
job a lot harder.
I need the analysis for Pottery Craft frit # 2954 - described as a
calcium/borate frit.
Thanks for any help you can give.
Best regards, RR
Ron Roy
93 Pegasus Trail
Scarborough, Ontario
Canada M1G 3N8
Tel: 416-439-2621
Fax: 416-438-7849
Web page: http://digitalfire.com/education/people/ronroy.htm
Alex Wilson on sat 17 apr 99
Hello Musa, I wonder if you have any other analyses handy, i.e. Podmore 2246?
I'm attempting to match a glaze from the U.K. using frits available here in
the U.S. from Ferro or Fusion.
T.I.A.
Alex
| |
|