Arturo M Devitalis on thu 15 apr 99
In a "Senior moment" I pitched out my kiln wash recipie...had alumina
hydrate plus? plus? & in ? proportions. TIA
(reply off-line if you wish)
___________________________________________________________________
You don't need to buy Internet access to use free Internet e-mail.
Get completely free e-mail from Juno at http://www.juno.com/getjuno.html
or call Juno at (800) 654-JUNO [654-5866]
Marvin Flowerman on fri 16 apr 99
Kiln wash a la Steven Branfman:
2 parts EPK
2 parts Flint
1 Part Alumina Hydrate
Works very well for me./
Good Luck!
Marvin Flowerman (marvpots@aol.com)
| |
|