Here is one I have:
Birke's Celadon ^5 to ^6
Feldspar 58
Whiting 17
Flint 14
Ball Clay 6
Zinc Oxide 5
Copper Oxide 1
Crazes on some of my clay bodies, but has a good fit on my ^6
porcelain, have (accidently) bounced a vase on my ceramic floor
several times and nary a chip or a crack, quite a pretty translucent
green.
Toni Martens, Durban South Africa, where a hot ,dry, mountain wind
has blown all day, leaving me with fried eyes and gritty mood.