Vince Pitelka on thu 22 apr 99
In the past few weeks there have been at least three glaze recipes posted on
Clayart without the firing temperature. Please folks, ALWAYS include the
cone number and the atmosphere WHENEVER you post a glaze recipe. Otherwise
it is completely useless to anyone who may have missed the original post
about the particular glaze. Thanks and best wishes -
- Vince
Vince Pitelka - vpitelka@DeKalb.net
Home 615/597-5376, work 615/597-6801, fax 615/597-6803
Appalachian Center for Crafts
Tennessee Technological University
1560 Craft Center Drive, Smithville TN 37166
| |
|