search  current discussion  categories  materials - misc 

analysis for minsilspar (minspar) from kraft chemical (supplier)

updated fri 7 may 99

 

Bruce Girrell on thu 6 may 99

For those who may be interested:

I ordered some Kona feldspar and the supply house substituted a product
called Minspar.
It wasn't in my Insight MDT, so I made a couple of calls and tracked down
the analysis.

SiO2 9.955 76.8%
Al2O3 1.069 14.0
Na2O 0.616 4.9
K2O 0.232 2.8
CaO 0.153 1.1
MgO Trace
Fe2O3 0.003 0.06

LOI 0.3

Kraft actually supplied the percentages and I converted to unity, so the
numbers to trust are the percentages.