Does anyone have a recipe for Copper Penney Raku? I've had a request and
can't find one in my books.

TIA,
Merrilee
merrileepots@juno.com

___________________________________________________________________
You don't need to buy Internet access to use free Internet e-mail.
Get completely free e-mail from Juno at http://www.juno.com/getjuno.html
or call Juno at (800) 654-JUNO [654-5866]

Dewitt Gimblet on wed 19 may 99

Merrilee,

Below is the recipe for Copper Penny. Lots more at
http://www.mdc.net/~rjwilt/info/DEGRaku.htm

deg

===================
Copper Penny Raku Glaze

Gerstley borate 80
Potash feldspar 20
Copper carbonate 2
Cobalt carbonate 1
Yellow Ochre 7

==================

At 01:15 PM 5/18/99 -0400, you wrote:
>----------------------------Original message----------------------------
>Does anyone have a recipe for Copper Penney Raku? I've had a request and
>can't find one in my books.
>
>TIA,
>Merrilee
>merrileepots@juno.com
>
>___________________________________________________________________
>You don't need to buy Internet access to use free Internet e-mail.
>Get completely free e-mail from Juno at http://www.juno.com/getjuno.html
>or call Juno at (800) 654-JUNO [654-5866]
>

Dennis Davis on thu 20 may 99

The Copper Penney I use is:

50 Custer Spar
80 Gerstley Borate
10 Copper Carbonate
5 Red Iron Oxide
145 Total

Dennis in Stafford, VA

Merrilee Pascaris wrote:
--------------------------Original message--------------------------
>Does anyone have a recipe for Copper Penney Raku?

Faye Clarke on thu 20 may 99

Do have a Raku glaze by a different but similiar name...as follows:
COINSPOT
1500 Gerstly Borate
176 Bone Ash
45 Cobalt Carbonate
85 copper Carb.. Large amount I know but can be cut down..

Mix== Strain through 80 mesh --on a dry finger should stick to hairs..
Best if left overnight before using...
Good luck from Faye in North Lotus Land... Van. Island Canada..
Just a side note... I have a daughter -- Marilee...



>----------------------------Original message----------------------------
>Does anyone have a recipe for Copper Penney Raku? I've had a request and
>can't find one in my books.
>
>TIA,
>Merrilee
>merrileepots@juno.com
>
>___________________________________________________________________
>You don't need to buy Internet access to use free Internet e-mail.
>Get completely free e-mail from Juno at http://www.juno.com/getjuno.html
>or call Juno at (800) 654-JUNO [654-5866]
>
>

Maggie Woodhead on thu 20 may 99

Kia Ora
The recipe I have is as follows:-

Colemanite-80
Cornish stone-20
Yellow Ochre-8
Black Copper Oxide-2
Cobalt Oxide-1

Good luck ----Best Wishes Maggie----
maggie@clear.net.nz

-----Original Message-----
From: Merrilee Pascaris
To: CLAYART@LSV.UKY.EDU
Date: Wednesday, 19 May 1999 05:16
Subject: Copper Penney Raku


----------------------------Original message----------------------------
Does anyone have a recipe for Copper Penney Raku? I've had a request
and
can't find one in my books.

TIA,
Merrilee
merrileepots@juno.com

___________________________________________________________________
You don't need to buy Internet access to use free Internet e-mail.
Get completely free e-mail from Juno at http://www.juno.com/getjuno.html
or call Juno at (800) 654-JUNO [654-5866]