Hanne Bjorklund on thu 6 may 99

Re: Glass, for effect.

Sometimes I put a few coloured glass pieces into a concave knob on top of
a lid. The glass always crazes. Is there something I can add, =sprinkle
among the glass bits that will eliminate the crazing? Like a frit?

We have really great green and blue wine-bottles in this land of upside
down, with colours that do not burn out at cone 6 oxidation.

HANNE