Mark Burleson on thu 6 may 99
----------------------------Original message----------------------------
Odyssey Center for the Ceramic Arts in Asheville, NC will host the
following workshops this summer. For more information, please re to
odyssey@interpath.com or phone 828.285.0210.
Dishin': Narrative Surface Decoration
with George Bowes
July 12 - 16, 1999
Workshop Description:
Using red earthenware clay, we will throw and handbuild simple
utilitarian forms. With colored slips and underglaze, we will embellish
our surfaces with stories from daily life - from the mundane to the
sensational. Work will be once fired to cone 03. In discussing the
finished objects, we will examine the role of table manners in the new
millennium.
| |
|