styrofoam thanks

updated tue 11 may 99

 

Barb Lund on fri 7 may 99

thanks to all who responded to my question bout burning out styrofoam in
the kiln. Everybody says NEVER and Tom Buck had the great idea of firing
out the piece in a grill or hibatchi- then firing the clay form that is
left. I'll p[ass this on to my scuptor pal and we shall see what he comes
up with! What would I do without this group!? Barb in Bloomington

hal mc whinnie on mon 10 may 99

you may wish to try to fire outdoors in a raku type kiln.
i have two old electric kiln converted to propane and fire salt and sodea
glazes with my raku ware.