I would appreciate your opinion on the following situation:

The temperature varies by one cone throughout a top-loading, 12 sided
electric kiln. However, during the last 100 degrees of firing,
temperature uniformity is very close.

Will the last 100 degrees of even temperature compensate for the
earlier uneven firing?