search  current discussion  categories  glazes - cone 8-10 

cone 10 blues

updated sat 22 may 99

 

Terry or Karen Mayo on fri 21 may 99

Hi Folks,
I'm new to Clayart and I'm looking forward to reading good stuff from
good people who love to pot.
I haven't been totally successful coming up with a nice dark blue matt
glaze that doesn't bleed pink or mauve, but has a good opaque blue
finish. The clay I'm using is Dillo White, ^10.
I could also use some help in ways to get uniform coverage on my pieces.
I'm currently dipping or pouring depending on the size of the piece. If
there is an address I can write for glaze recipes, I'd appreciate that
information too. Thanks so much.
Karen from houston