Brian Crocker on fri 21 may 99
G'Day Dirk,
Yes you can make your own paper clay. Not as expensive as the prepared version
from the Potter's Store.
Have a look at http://www.paperclayart.com
Have lived in Gelgium {Bruxelles} lovely country, friendly people.
I have an 'Attachment' on it [Paper clay] if you need it let me know.
Kind regards, Brian C..
At 05:22 PM2:10: 19/05/99 EDT, you wrote:
>----------------------------Original message----------------------------
>Hi, Im there again the Belgian potter. i heard a lot of paperclay, but I'm =
>never
>have worked with it. Can you make it yourself and how do you work with it. =
>Are
>there different way? How do you fire it.
>I have a huge selfmade gaskiln.
>
>
Brian Crocker.
4 Erica Street,
Tea Tree Gully 5091,
South Australia. [e.mail] crocker@dove.net.au
With them the Seed of Wisdom did I sow,
And with my own hand labour'd it to grow:
And this was all the Harvest that I reap'd --
"I came like Water, and like Wind I go." The Rubaiyat.
Edouard Bastarache on sat 22 may 99
------------------
Hello all,
you can also check http://www.paperclay.co.uk/index.html
it is Michael Downey's URL
Later,
Edouard Bastarache
edouardb=40sorel-tracy.qc.ca
http://www.sorel-tracy.qc.ca/=7Eedouardb/
-----Message d'origine-----
De : Brian Crocker =3Ccrocker=40dove.net.au=3E
=C0 : CLAYART=40LSV.UKY.EDU =3CCLAYART=40LSV.UKY.EDU=3E
Date : 21 mai, 1999 10:14
Objet : Re: Paper clay, can you make it yourself
----------------------------Original message----------------------------
G'Day Dirk,
Yes you can make your own paper clay. Not as expensive as the prepared
version
from the Potter's Store.
Have a look at http://www.paperclayart.com
Have lived in Gelgium =7BBruxelles=7D lovely country, friendly people.
I have an 'Attachment' on it =5BPaper clay=5D if you need it let me know.
Kind regards, Brian C..
At 05:22 PM2:10: 19/05/99 EDT, you wrote:
=3E----------------------------Original message----------------------------
=3EHi, Im there again the Belgian potter. i heard a lot of paperclay, but =
I'm
=3D
=3Enever
=3Ehave worked with it. Can you make it yourself and how do you work with =
it.
=3D
=3EAre
=3Ethere different way? How do you fire it.
=3EI have a huge selfmade gaskiln.
=3E
=3E
Brian Crocker.
4 Erica Street,
Tea Tree Gully 5091,
South Australia. =5Be.mail=5D crocker=40dove.net.au
With them the Seed of Wisdom did I sow,
And with my own hand labour'd it to grow:
And this was all the Harvest that I reap'd --
=22I came like Water, and like Wind I go.=22 The Rubaiyat.
| |
|