Hello. Can anyone give me the formulas of nephelyne syenite and gerstley
borate? They don't seem to be in the Czech-English dictionary. Thank yoou.
j-m
Prague,CZ

DinaH on tue 25 may 99

This is what I have:
Gerstley Borate Na20 .133 Al2O3 1.0 SiO2 .406
Molecular wgt. 229
CaO .7 Fe2O3 Trace
MgO .167 B2O3 .947 L.O.I. 4.68

Neph Sye K2O .22 Al2O3 1.03 SiO2 4.55
Molecular wgt. 450.5
Na2O .71
CaO .06 Fe2O3 .002 L.O.I. .175

MgO .01
Dinah
JCJM wrote:

> ----------------------------Original message----------------------------
> Hello. Can anyone give me the formulas of nephelyne syenite and gerstley
> borate? They don't seem to be in the Czech-English dictionary. Thank yoou.
> j-m
> Prague,CZ

L Ewing on tue 25 may 99

Hi j-m,

You can obtain the formulae for these materials from the materials listing at th

http://www.tekotago.ac.nz/art/matrixgoweb/default.htm


Lawrence Ewing

Senior Lecturer in Ceramics
School of Art
Otago Polytechnic

lewing@clear.net.nz

21 Slant St
Careys Bay
Dunedin
NEW ZEALAND

ph 03 472 8801

Author of Matrix Glaze Calculation Software for Macintosh & Windows95

Web site URL:

http://www.tekotago.ac.nz/art/matrixgoweb/default.htm


-----Original Message-----
From: JCJM [SMTP:jcjm@terminal.cz]
Sent: Tuesday, May 25, 1999 1:54 AM
To: CLAYART@LSV.UKY.EDU
Subject: don't know formulas

----------------------------Original message----------------------------
Hello. Can anyone give me the formulas of nephelyne syenite and gerstley
borate? They don't seem to be in the Czech-English dictionary. Thank yoou.
j-m
Prague,CZ

Frank Gaydos on wed 26 may 99

Gerstley Borate Na2O-2CaO-5B2O3-8H2O
Nepheline Syenite Na2O-Al2O3-2SiO2


Frank Gaydos
510 Gerritt St.
Philadelphia,Pa.
19147-5821 USA

fgaydos@erols.com
http://www.erols.com/fgaydos
http://www.members.xoom.com/fgaydos/
----- Original Message -----
From: JCJM
To:
Sent: Monday, May 24, 1999 7:54 AM
Subject: don't know formulas


> ----------------------------Original message----------------------------
> Hello. Can anyone give me the formulas of nephelyne syenite and gerstley
> borate? They don't seem to be in the Czech-English dictionary. Thank yoou.
> j-m
> Prague,CZ
>