search  current discussion  categories  kilns & firing - manufacturers 

orfice size for alpine

updated sat 5 jun 99

 

Bryan Hannis on thu 3 jun 99

Hi

Does anyone know the right orfice size for a alpine HF 24 for propane fuel,
and how many orfices per burner??

Bryan Hannis

Nils Lou on fri 4 jun 99

If you have the original alpine burner with the pipe nipple going through
the burner tube it is usually set with three holes in a row. For propane
put in a new nipple and drill three #51 holes 1/4" apart. NL

On Thu, 3 Jun 1999, Bryan Hannis wrote:

> ----------------------------Original message----------------------------
> Hi
>
> Does anyone know the right orfice size for a alpine HF 24 for propane fuel,
> and how many orfices per burner??
>
> Bryan Hannis
>