loose bricks/trowel eze.2

updated sun 30 may 99

 

mel jacobson on sat 29 may 99

lesley.
you would be better served if you just jacked up that spot in your arch.
then replace the broken offenders. i hate broken key bricks.
(that is why i fire in flattops.)

or:
slather the piece with trowl eze and patch back together.
as i said yesterday, it works best, so far, in my repair time
on earth.

trowl eze is a brand name from thermal ceramics.
check brick dealers for avail.
mel/mn
think of all the bar b que that will spill down chins this weekend.
hell, fire pots in those b b q's as you do the chicken.
good ol` barium chicken. nice red/brown glaze.