search  current discussion  categories  glazes - specific colors 

green / bronze metal patina

updated sat 26 jun 99

 

muddpie on fri 25 jun 99

Barbara or anyone else in the know...

would you have that bronze metal patina also? and I am going to assume that it
was also a ^6 ox. glaze?

thanks so much...
Julie in michigan

Barbara Lewis wrote:

> ----------------------------Original message----------------------------
> This is not food safe. It appeared about five years ago in CM with Bronze
> Metal Patina. Neither are food safe. Barbara
>
> At 09:01 AM 6/23/99 EDT, you wrote:
> >----------------------------Original message----------------------------
> >Would this be a food safe glaze??? I still am learning much from all the
> >comments on ClayART... Anyone care to send us some warm weather up here to
> >Vancouver Island --sure would help bring on the tourists... they don't seem
> >to like it any better than we do. To good Potting.. Faye..
> >
> >At 08:47 AM 6/22/99 EDT, you wrote:
> >>----------------------------Original message----------------------------
> >>Here's one, published in DonGoodrich's list
> >>
> >>================================
> >>REYNOLDS GREEN METAL PATINA (^6 OX) tested well: widely varied shades of
> >>blue &
> >>Copper Carbonate 2.44 green w varying surfaces
> >>Lithium Carbonate 39.02
> >>Ferro Frit 3124 29.27
> >>Superpax 19.51
> >>Flint 9.76
> >>================================
> >> Hope this helps
> >>
> >>
> >>
> >>
> >>
> >>At 11:23 AM 6/20/99 EDT, you wrote:
> >>>----------------------------Original message----------------------------
> >>>Hi all,
> >>>
> >>>I'm looking for a glaze from a couple of years ago that was in Ceramics
> >>>Monthly called Green Patina. It was a cone 6 glaze and was in an article on
> >>>texture or special effects glazes. Anybody know off hand what this is?
> >>>
> >>>TIA,
> >>>
> >>>Peter Atwood
> >>>
> >>>
> >>>_______________________________________________________________
> >>>Get Free Email and Do More On The Web. Visit http://www.msn.com
> >>>
> >>>
> >>
> >>
> >
> Wellspring Clayworks
> 5412 Well Spring Road
> La Plata, MD 20646
> blewis@crosslink.net
> (301) 932-3915