another terra cotta question

updated sat 3 jul 99

 

Phyllis Gibson on thu 1 jul 99

'I've also started working in a very little terra cotta. I applied a
> clear glaze and it turns so dark and I prefer the real terra cotta
> color....I fired the terra cotta to only 04 bisque.

Does anyone know about white washing that could be posted to entire list or
perhaps various shades of slip that would make an interesting piece?

Does Duncan make anything premixed?

Thank you.

Jackie Richards on fri 2 jul 99

I am just a beginner, but didnt I read somewhere where you can use kiln wash
as a whitish glaze for terra cotta that just leaves a white hazy look?