Barbara Lewis on fri 2 jul 99
Does anyone on the list use Laguna's Danish White w/sand. I'm interested in
finding a light-firing stoneware body and this was recommended to me. I'll
be using the clay for throwing small, medium and large forms. Any comments
would be appreciated. Thanks, Barbara
Wellspring Clayworks
5412 Well Spring Road
La Plata, MD 20646
blewis@crosslink.net
(301) 932-3915
Wendy Hampton on sat 3 jul 99
Hi,
I used Danish White for a few years. It has great elasticity and is easy
throwing. I also used it for Raku and it worked for that also.
Wendy
| |
|