tmartens on wed 30 jun 99

Hi Antoinette
The closest you are going to get to the South African Ferro Fritt 510
will be Ferro 3134 and if any of your old recipes used Colemanite you
can sub with Gerstley Borate and EPK is what is called Selena here in
the 'other South'
Toni happy it is still 'winter' in Durban South Africa

> ----------------------------Original message----------------------------
>
> Lori asked why I do not simply carry on with my old recipes. I whish I
> could. I sold my studio in South Africa that was worth thousands of
> rands (SA money) and was build up over almost 20 years. The shipping
> to America is to expensive. It is also too time consuming. It will take
> almost six weeks for me to get basic ingredients from SA to the US.
> Learning about new raw materials and substitutes can also be exciting.
> By the way will I find Ferro fritt 510 somewhere here? I did not see it
> in any catalog jet.
>
> Antoinette.
>
>
> ===
> Antoinette Badenhorst
> PO Box 552
> Saltillo,Mississippi
> 38866
> Telephone (601) 869-1651
> timakia@yahoo.com
> _________________________________________________________
> Do You Yahoo!?
> Get your free @yahoo.com address at http://mail.yahoo.com