Kathleen Ristinen Jonas on mon 19 jul 99
brand: WRAP; made by Worden Robinson Art Pottery, Sperryville, VA
22740
type: updraft, gas (either LP or natural), cone 10, round, top loading
exterior: 32" across, 35" high, including firebrick lid, galvanized
metal jacket
interior: 26" high, 23.5 inches across, firebrick
capacity: 7 cubic feet (approximately)
kiln walls are 4" in thickness
burner: one #2 Buzzer
included: 9" extension ring (for bisque firings); 4 cordierite half
shelves; 2 full shelves
condition: very good to excellent; fired twice only
price: $625
available: after August 6 when I return from a trip to Finland
location: 190 miles northwest of Minneapolis, MN
reason for selling: prefer my homemade downdraft kiln
I will be off this list soon, so please e-mail directly or telephone:
218-564-4299
| |
|