search  current discussion  categories  glazes - other named glazes 

robert sperry lichen glazes

updated tue 27 jul 99

 

Elca Branman on thu 15 jul 99

A colleague , without access to Clayart , has asked me to request any
Robert Sperry Crawling glaze for cone 10.Thanks as usual, to all who are
generous with their knowledge.
Elca.. at home in Sarasota,Florida,USA

___________________________________________________________________
Get the Internet just the way you want it.
Free software, free e-mail, and free Internet access for a month!
Try Juno Web: http://dl.www.juno.com/dynoget/tagj.

Gregory D Lamont on sun 25 jul 99

At 09:21 AM 7/15/99 -0400, you wrote:
>----------------------------Original message----------------------------
>A colleague , without access to Clayart , has asked me to request any
>Robert Sperry Crawling glaze for cone 10.Thanks as usual, to all who are
>generous with their knowledge.
>Elca.. at home in Sarasota,Florida,USA
>
>___________________________________________________________________
>Get the Internet just the way you want it.
>Free software, free e-mail, and free Internet access for a month!
>Try Juno Web: http://dl.www.juno.com/dynoget/tagj

Elca,
Don't know if you've already received this as I'm a little late responding to
the original post.

Sperry Crawl Glaze

Nepheline Syenite 65
Magnesium Carbonate 25
Ball Clay 10

For color add: 10% stain. Good over black engobe.