Tom -

You can fire paperclay to whatever Cone the clay body you are using
fires at. You will have to experiment with the amount of paper in the mix
depending on how smooth your friend wants their sculpture to be. It will get
rid of the cracks and the warping and the weight. I have not yet found any
clay body that it does not work well with. I love the stuff.