Sharon R Pemberton on mon 2 aug 99

Do you get black core?

Bob Hanlin on wed 4 aug 99

Uh, no. My clay body contains so little iron that it's not a problem.
Come to think about it sometimes I have some reqular stoneware in the kiln
too and it may black core...never broke a piece to check.