Charles and Tamara Schulz on mon 9 aug 99

Thanks everyone for helping me contact geil. I couldn't seem to get
through the server, but finally have made it on one of the addresses you sent.
I'm planning to order a new kiln for our art center, but in the mean time I
DESPARATELY need to fix the existing one. It's a fiber lined front loading
gas kiln. The fiber ceiling is sagging down and chunks are falling off.
How should I go about replacing it? I have NO idea how to repair a kiln.

PLEASE HELP!!!

Tamara--in Okinawa. If your planning to tour Japanese potteries, you MUST
see the treasures we have here!!