Lesley Alexander on fri 6 aug 99
Try Sycamore White. That should be in the archives, but:
^10 reduction works fine, why not oxidation?:
Whiting 18.19
Custer 50.19
Flint 19.07
Zircopax 25.47
Lesley in So Calif.
Bonita Cohn on sun 8 aug 99
Here's a fat white glaze, thin or thick, no runs, collected at the Maryland
Institute in 70's:
DIME STORE WHITE
custer spar 75
talc 10
kaolin 10
zircopax 5
----------------------
100 Takes stains well.
Bonita in misty, cool San Francisco
http://cpmg.com/anagama
http://silverhawk.com/ex99/cohn
Pamala Browne on mon 9 aug 99
hi bonita is that ^10 white reduction or oxidation???
----- Original Message -----
From: Bonita Cohn
To:
Sent: Sunday, August 08, 1999 3:50 PM
Subject: Re: Glaze Wanted, white ^10
> ----------------------------Original message----------------------------
> Here's a fat white glaze, thin or thick, no runs, collected at the
Maryland
> Institute in 70's:
> DIME STORE WHITE
> custer spar 75
> talc 10
> kaolin 10
> zircopax 5
> ----------------------
> 100 Takes stains well.
>
> Bonita in misty, cool San Francisco
> http://cpmg.com/anagama
> http://silverhawk.com/ex99/cohn
>
| |
|