search  current discussion  categories  kilns & firing - coatings 

old fibre/itc

updated sun 8 aug 99

 

mel jacobson on sat 7 aug 99

we have found that when you spray itc 100 on fibre you have to compress
it very hard before you spray.
feriz say's....run over it with a tractor...flat as you can.
when the spray is applied, it will come back to it's original thickness.
that is what we did when we built the salt kiln at the farm. when you
laminate/or tile your kiln, you must get those tiles of fibre flat.

this adds lagitimacy to what don is talking about....old fibre has spread
out...it is falling down...so when you spray the itc, the weight increases
that gap.
mel/mn
http://www.pclink.com/melpots
from minnetonka, minnesota, u.s.a.