Bonita Cohn on tue 10 aug 99


hi bonita is that ^10 white reduction or oxidation???
The firings were reduction. Hardly a spot, on iron bearing clay, (well maybe
some) thru its opaque cover. Probably would be fine in oxidation, too.
> Here's a fat white glaze, thin or thick, no runs, collected at the Maryland
Institute in 70's:
> DIME STORE WHITE
> custer spar 75
> talc 10
> kaolin 10
> zircopax 5
> ----------------------
> 100 Takes stains well.