hasebe on tue 10 aug 99
Hi, I found a bag of Gerstley Borate, which had been soaked with water last
year by accident for a week. The Gerstley Borate is now completely dry. Is
its property the same or has been changed in regards to use as glaze
material?
Hodaka Hasebe
hasebeh@rochester.rr.com (Hodaka Hasebe)
Pittsford, NY
716-264-9698
Frank Gaydos on thu 12 aug 99
Chances are it is different. Best way to find out is to fire a test using
the GB and compare it, see if the glaze looks different.
----- Original Message -----
From: hasebe
To:
Sent: Tuesday, August 10, 1999 12:05 PM
Subject: Once Soaked Gerstley Borate question
> ----------------------------Original message----------------------------
>
> Hi, I found a bag of Gerstley Borate, which had been soaked with water
last
> year by accident for a week. The Gerstley Borate is now completely dry.
Is
> its property the same or has been changed in regards to use as glaze
> material?
>
>
>
> Hodaka Hasebe
> hasebeh@rochester.rr.com (Hodaka Hasebe)
> Pittsford, NY
> 716-264-9698
| |
|